Raex® AR500
Download data sheet
Download data sheet
Product type | Thickness 1) (mmin) |
Width 1) (mmin) |
Length 1) (mmin) |
Hardness 2) (HBW) |
Typical yield strength (MPaksi), not guaranteed |
Typical tensile strength (MPaksi), not guaranteed |
Typical Elongation A (%),not guaranteed |
---|---|---|---|---|---|---|---|
Sheet | 3.00 - 7.000.118 - 0.276 | 1000 - 172539.370 - 67.913 | 2000 - 1200078.740 - 472.440 | 470 - 540 | 1400203 | 1650239 | 8 |
Plate | 6.00 - 20.000.236 - 0.787 | 1000 - 320039.370 - 125.984 | 2000 - 1200078.740 - 472.440 | 470 - 540 | 1300188 | 1600232 | 8 |
Plate | 20.01 - 40.000.788 - 1.575 | 1000 - 320039.370 - 125.984 | 2000 - 1200078.740 - 472.440 | 450 - 540 | 1300188 | 1600232 | 8 |
Plate | 40.01 - 80.001.575 - 3.150 | 2000 - 250078.740 - 98.425 | 4000 - 9500157.480 - 374.015 | 450 - 540 | 1300188 | 1600232 | 8 |
1) More detailed information on dimensions is provided from RaexSmart. Please contact your local sales representant for more information.
2) Brinell Hardness is measured, according to EN ISO 6506-1 on milled surface 0.3-3.0mm below surface. Hardness value is being announced in the material certificate. Mechanical properties are tested in transverse direction and tabulated for information only and values are not shown in material certificate.
Product | Longitudinal test, typical impact energy, Charpy V 10x10 mm test specimen 1) |
---|---|
Raex® AR 500 sheet & plate | 30 J / -40 °C22 ft-lbs / -40 °F |
1) Impact testing according to EN ISO 148-1 is performed on thickness ≥6mm. The specific value corresponds to a full-size specimen. Impact values are tabulated for information only and value are not shown in material certificate.
Product type | C (max %) |
Si (max %) |
Mn (max %) |
P (max %) |
S (max %) |
Cr (max %) |
Ni (max %) |
Mo (max %) |
B (max %) |
---|---|---|---|---|---|---|---|---|---|
Sheet | 0.27 | 0.50 | 1.60 | 0.025 | 0.010 | 1.20 | 1.00 | 0.25 | 0.005 |
Plate | 0.30 | 0.80 | 1.70 | 0.025 | 0.015 | 1.50 | 1.00 | 0.50 | 0.005 |
The steel is grain refined.
Product type | Sheet | Plate | Plate | Plate | Plate |
---|---|---|---|---|---|
Thickness (mmin) | 3.00 - 7.000.098 - 0.276 | 6.00 - 20.000.236 - 0.787 | 20.01 - 32.000.787 - 1.260 | 32.01 - 52.001.260 - 2.047 | 52.01 - 80.002.048 - 3.150 |
Typ CET(CEV) 1) | 0.40 (0.55) | 0.40 (0.51) | 0.41 (0.59) | 0.43 (0.65) | 0.43 (0.68) |
1) The CEV value is being announced in the inspection certificate and the CET values are tabulated for information only.
Plates tolerances according to EN 10029 Class A, tighter tolerances upon agreement. Sheets tolerances according to EN 10051 Category A.
For plate tolerances according to EN 10029, tighter tolerances upon agreement. Sheets tolerances according to EN 10051.
Tolerances according to EN 10029 for plate and according to EN 10051 for sheet.
For plate and sheet the flatness deviation is max 6 mm/m.
According to EN 10163-2 Class A, Subclass 3.
Minimum inner bending radii for a 90° bend are:
Sheets, 3.5 x t (transverse) and 4 x t (longitudinal).
Plates t ≤ 20 mm, 5 x t (transverse) and 6 x t (longitudinal).
The delivery condition is quenched. Sheets are available in as rolled surface condition with mill edge. Plates are available in as-rolled or shopprimed surface condition. Delivery requirements can be found in SSAB´s brochure at www.raexsteel.com.
Welding, bending and machining recommendations can be found in brochures at www.raexsteel.com or consult Tech Support.
Raex® AR is not intended for further heat treatment. Mechanical properties are achieved by quenching. The properties of the delivery condition cannot be retained after exposure to temperatures in excess of 250°C.
Appropriate health and safety precautions must be taken when welding, cutting, grinding or otherwise working on this product. Grinding, especially of primer coated plates, may produce dust with a high particle concentration.